Quantitative fractography of 2205 duplex stainless steel after a sulfide stress cracking test

✍ Scribed by Katarzyna Klyk-Spyra; Maria Sozańska


Book ID
113779926
Publisher
Elsevier Science
Year
2006
Tongue
English
Weight
326 KB
Volume
56
Category
Article
ISSN
1044-5803

No coin nor oath required. For personal study only.


📜 SIMILAR VOLUMES


The effect of shot peening on stress cor
✍ Y.F. Al-Obaid 📂 Article 📅 1995 🏛 Elsevier Science 🌐 English ⚖ 509 KB

In this paper an attempt has been made to study the effect of shot peening on stress corrosion cracking of 2205-Duplex stainless steel. Cast steel shot was selected to be the peening media. Specimens of 2205-Duplex stainless steel were tested in the peened and unpeened condition. Quantitative data o

Field and laboratory experiences of Sulf
✍ Bruno Bazzoni; Alberto Cigada; Luciano Lazzari; Pietro Pedeferri 📂 Article 📅 1985 🏛 John Wiley and Sons 🌐 German ⚖ 745 KB

Targets of this work have been: testing of duplex stainless steel in field (into a geothermal well) and in laboratory NACE environment in presence of crevices and sharp defects; development of testing based on fracture mechanics and comparison with traditional testing approach. The following types