Stress corrosion cracking of 2205 duplex stainless steel in H2S–CO2environment
✍ Scribed by Z. Y. Liu; C. F. Dong; X. G. Li; Q. Zhi; Y. F. Cheng
- Book ID
- 106394883
- Publisher
- Springer
- Year
- 2009
- Tongue
- English
- Weight
- 737 KB
- Volume
- 44
- Category
- Article
- ISSN
- 0022-2461
No coin nor oath required. For personal study only.
📜 SIMILAR VOLUMES
In this paper an attempt has been made to study the effect of shot peening on stress corrosion cracking of 2205-Duplex stainless steel. Cast steel shot was selected to be the peening media. Specimens of 2205-Duplex stainless steel were tested in the peened and unpeened condition. Quantitative data o
The dynamical processes of the nucleation and propagation of stress corrosion cracking (SCC) of low-alloy steels with a wide range of tensile strength in gas and aqueous solution of HZ.7 were followed metallographically by using a polished WOL type constant deflection specimen. The results show that