𝔖 Bobbio Scriptorium
✦   LIBER   ✦

Stress Corrosion Cracking of Welded 2205 Duplex Stainless Steel in Sulfide-containing Caustic Solution

✍ Scribed by Ananya Bhattacharya; Preet M. Singh


Book ID
107462668
Publisher
Springer US
Year
2007
Tongue
English
Weight
466 KB
Volume
7
Category
Article
ISSN
1547-7029

No coin nor oath required. For personal study only.


πŸ“œ SIMILAR VOLUMES


The effect of shot peening on stress cor
✍ Y.F. Al-Obaid πŸ“‚ Article πŸ“… 1995 πŸ› Elsevier Science 🌐 English βš– 509 KB

In this paper an attempt has been made to study the effect of shot peening on stress corrosion cracking of 2205-Duplex stainless steel. Cast steel shot was selected to be the peening media. Specimens of 2205-Duplex stainless steel were tested in the peened and unpeened condition. Quantitative data o

Determination of corrosion-assisted stre
✍ A. DΓ­az-SΓ‘nchez; V. M. CastaΓ±o πŸ“‚ Article πŸ“… 2007 πŸ› John Wiley and Sons 🌐 German βš– 209 KB πŸ‘ 1 views

The corrosion assisted stress crack growth rate of 304L stainless steel welds, was determined by the rising displacement test method. The experiments were carried out in a Boiling Water Reactor (BWR) environment, using a refreshed autoclave loop system at 288 C and 8 MPa of pressure. Pre-fatigued CT