๐”– Bobbio Scriptorium
โœฆ   LIBER   โœฆ

Critical Stress for Stress Corrosion Cracking of Duplex Stainless Steel in Sour Environments

โœ Scribed by Miyasaka, A.; Kanamaru, T.; Ogawa, H.


Book ID
121246924
Publisher
NACE International
Year
1996
Tongue
English
Weight
488 KB
Volume
52
Category
Article
ISSN
0010-9312

No coin nor oath required. For personal study only.


๐Ÿ“œ SIMILAR VOLUMES