## Abstract Stress corrosion crack velocity and stress corrosion threshold stress intensity have been measured for 18Crβ10Niβ0,5Ti stainless steel in relation to environmental variations. These studies showed that both stage I and stage II growth rate dependence on K are influenced by environmental
Stress corrosion cracking of stainless steel used in drill collars
β Scribed by N.A. Mariano; D. Spinelli
- Publisher
- Elsevier Science
- Year
- 2004
- Tongue
- English
- Weight
- 886 KB
- Volume
- 385
- Category
- Article
- ISSN
- 0921-5093
No coin nor oath required. For personal study only.
π SIMILAR VOLUMES
## Abstract In one of the gas processing facilities in Abu Dhabi, UAE; a case of 316L stainless steel material failure occurred in the fractionating column due to stress cracking corrosion twice in a cycle of less than 2βyears. This paper studies the stress corrosion cracking behavior of the 316L s
The dynamical processes of the nucleation and propagation of stress corrosion cracking (SCC) of low-alloy steels with a wide range of tensile strength in gas and aqueous solution of HZ.7 were followed metallographically by using a polished WOL type constant deflection specimen. The results show that