𝔖 Bobbio Scriptorium
✦   LIBER   ✦

Growth of manganese oxide thin films by atomic layer deposition

✍ Scribed by O. Nilsen; H. Fjellvåg; A. Kjekshus


Book ID
108388753
Publisher
Elsevier Science
Year
2003
Tongue
English
Weight
657 KB
Volume
444
Category
Article
ISSN
0040-6090

No coin nor oath required. For personal study only.


📜 SIMILAR VOLUMES


Atomic Layer Deposition of Gadolinium Ox
✍ K. Kukli; T. Hatanpää; M. Ritala; M. Leskelä 📂 Article 📅 2007 🏛 John Wiley and Sons 🌐 English ⚖ 320 KB 👁 1 views

Thin cubic Gd 2 O 3 films are grown by atomic layer deposition (ALD), in the temperature range 300-400 °C, using a novel tris(2,3-dimethyl-2-butoxy)gadolinium(III) precursor, Gd[OC(CH 3 ) 2 CH(CH 3 ) 2 ] 3 , and water. The films are crystalline in their as-deposited state. The films contain some res