๐”– Bobbio Scriptorium
โœฆ   LIBER   โœฆ

Berkovich Nanoindentation on AlN Thin Films

โœ Scribed by Sheng-Rui Jian; Guo-Ju Chen; Ting-Chun Lin


Book ID
107470705
Publisher
Springer-Verlag
Year
2010
Tongue
English
Weight
383 KB
Volume
5
Category
Article
ISSN
1931-7573

No coin nor oath required. For personal study only.


๐Ÿ“œ SIMILAR VOLUMES


Berkovich nanoindentation and deformatio
โœ Chien-Huang Tsai; Sheng-Rui Jian; Jenh-Yih Juang ๐Ÿ“‚ Article ๐Ÿ“… 2008 ๐Ÿ› Elsevier Science ๐ŸŒ English โš– 563 KB

The deformation mechanisms of GaN thin films obtained by metal-organic chemical vapor deposition (MOCVD) method were studied using nanoindentation with a Berkovich diamond indenter, micro-Raman spectroscopy and the cross-sectional transmission electron microscopy (XTEM) techniques. Due to the sharpn

Berkovich nanoindentation on InP
โœ Sheng-Rui Jian; Jason Shian-Ching Jang ๐Ÿ“‚ Article ๐Ÿ“… 2009 ๐Ÿ› Elsevier Science ๐ŸŒ English โš– 557 KB