## Abstract The general techniques necessary to produce a highβquality crossβsectioned ceramic specimen for transmission electron microscope observation are outlined. A particularly important point is that the width of the glued region between faces of the ceramic specimen must be < 0.2 ΞΌm to preve
Ion-machining ceramics for transmission electron microscopy
β Scribed by D.J. Gould
- Publisher
- Elsevier Science
- Year
- 1973
- Weight
- 287 KB
- Volume
- 6
- Category
- Article
- ISSN
- 0026-0800
No coin nor oath required. For personal study only.
π SIMILAR VOLUMES
During the microstructural examination of ceramic thermal barrier coatings by transmission electron microscopy (TEM), initial efforts for the preparation of cross-sectional thin foils from interface regions by conventional means were mostly failures. Delamination of the Yz03-stabilized ZrOz ceramic
Chew and C u l l i s (1984; 1985) have r e p o r t e d s u c c e s s f u l i o c m i l l i n g of InP and InP devices u s i n g i o d i n e as t h e r e a c t i v e gas. The i o d i n e i o n s n o t only s p u t t e r atoms from t h e s u r f a c e , b u t a l s o chemically r e a c t w i t h t're