The dissolution of the anodic oxide film formed on antimony in NaF solutions was investigated as a function of the fluoride ion concentration, formation voltage, and temperature using impedance and potential measurements. The rate of dissolution of the entire oxide film was found to follow a first o
Electrochemical behaviour of the antimony electrode in sulphuric acid solutions—I. Corrosion processes and anodic dissolution of antimony
✍ Scribed by D. Pavlov; M. Bojinov; T. Laitinen; G. Sundholm
- Publisher
- Elsevier Science
- Year
- 1991
- Tongue
- English
- Weight
- 640 KB
- Volume
- 36
- Category
- Article
- ISSN
- 0013-4686
No coin nor oath required. For personal study only.
✦ Synopsis
The corrosion processes at open circuit conditions and in the active dissolution region of antimony, at low anodic overpotentials, have been studied in sulphuric acid solutions. It was established that antimony dissolution at open circuit is coupled to oxygen reduction, which occurs via the hydrogen peroxide route. The rate of antimony dissolution was found to increase linearly with increasing acid concentration. Based on potentiodynamic, galvanodynamic and steady-state measurements as well as ac impedance data possible mechanisms for the corrosion processes at open circuit as well as for the dissolution of antimony in the active region are proposed and discussed.
📜 SIMILAR VOLUMES
Rmgdlsc voltammetrlc experiments on antimony m H,SO, solutions show that a partly passlvatmg oxide layer IS formed on the metal surface preventmg oxygen evolution Due to the Ionic conductlvlty and/or porosity of the layer the dlssolutlon of the metal proceeds through the layer, and Its rate 1s contr
The electrochemical behaviour and corrosion of lead in various concentrations of acetic, lactic (0É01 MÈ1É0 M), oxalic and tartaric (0É01 MÈ0É15 M) acid solutions were studied at 25¡C by a potentiodynamic method. The lead anode is readily soluble both in acetic and lactic acid solutions up to 2000 m
Kinetic parameters related to the anodic and cathodic processes in the electrolysis of fuming sulphuric acids on bright platinum and platinii platinum electrodes have been established, the electrolyte bemg kept at rest. Experiments cover temperatures from 25 to 70°C and oleums with a stdphur trioxtd