Acrylamide Polymerized in the Presence of Surfactants: Surface Analysis Using Atomic Force Microscopy

✍ Scribed by Chakrapani, Mukundan; Van Winkle, David H.; Patterson, Brian C.; Rill, Randolph L.


Book ID
126227700
Publisher
American Chemical Society
Year
2002
Tongue
English
Weight
153 KB
Volume
18
Category
Article
ISSN
0743-7463

No coin nor oath required. For personal study only.


πŸ“œ SIMILAR VOLUMES


Surfactants in heterophase polymerizatio
✍ S. Lam; A. C. Hellgren; M. SjΓΆberg; K. Holmberg; H. A. S. Schoonbrood; M. J. Unz πŸ“‚ Article πŸ“… 1997 πŸ› John Wiley and Sons 🌐 English βš– 353 KB πŸ‘ 2 views

Film formation of three different latices was studied using atomic force microscopy. The latices were made from a mixture of butyl acrylate, styrene, and acrylic acid using either a polymerizable or an unreactive anionic surfactant as an emulsifier. Sodium 11-crotonoyloxyundecan-1-ylsulfate and sodi