ZnO films grown by atomic layer deposition for organic electronics

✍ Scribed by Luka, Grzegorz; Godlewski, Marek; Guziewicz, Elzbieta; Stakhira, Pavlo; Cherpak, Vladyslav; Volynyuk, Dmytro