Transmission X-ray diffraction of single-crystal nickel-base superalloys

✍ Scribed by H. Biermann; B. Von Grossmann


Book ID
107449840
Publisher
The Minerals, Metals & Materials Society
Year
1999
Tongue
English
Weight
226 KB
Volume
30
Category
Article
ISSN
1073-5623

No coin nor oath required. For personal study only.


πŸ“œ SIMILAR VOLUMES


Synchrotron tomography of porosity in si
✍ T. Link; S. Zabler; A. Epishin; A. Haibel; M. Bansal; X. Thibault πŸ“‚ Article πŸ“… 2006 πŸ› Elsevier Science 🌐 English βš– 550 KB

Porosity in the single-crystal nickel-base superalloys CMSX-6, SRR99, CMSX-4 and CMSX-10 was investigated by synchrotron X-ray tomography, supplying information about the three dimensional distribution of pores and a statistical database of pore sizes and shapes. Tomography investigations were compl

X-ray topography and crystal orientation
✍ A. Onyszko; W. Bogdanowicz; K. Kubiak; J. Sieniawski πŸ“‚ Article πŸ“… 2010 πŸ› John Wiley and Sons 🌐 English βš– 327 KB

## Abstract A study of the crystal orientation and structural perfection of single crystal blades obtained by Bridgeman method from CMSX‐4 nickel superalloy at various withdrawal rates between 1 and 5 mm/min was carried out using the Laue diffraction method and X‐ray diffraction topography methods