Rafting in single crystal nickel-base superalloys — An overview

✍ Scribed by M. Kamaraj


Book ID
110649297
Publisher
Indian Academy of Sciences
Year
2003
Tongue
English
Weight
367 KB
Volume
28
Category
Article
ISSN
0256-2499

No coin nor oath required. For personal study only.


📜 SIMILAR VOLUMES


Synchrotron tomography of porosity in si
✍ T. Link; S. Zabler; A. Epishin; A. Haibel; M. Bansal; X. Thibault 📂 Article 📅 2006 🏛 Elsevier Science 🌐 English ⚖ 550 KB

Porosity in the single-crystal nickel-base superalloys CMSX-6, SRR99, CMSX-4 and CMSX-10 was investigated by synchrotron X-ray tomography, supplying information about the three dimensional distribution of pores and a statistical database of pore sizes and shapes. Tomography investigations were compl