๐”– Bobbio Scriptorium
โœฆ   LIBER   โœฆ

Single crystal elastic constants of two nickel based superalloys

โœ Scribed by D. P. Dandekar; A. G. Martin


Publisher
Springer
Year
1989
Tongue
English
Weight
156 KB
Volume
8
Category
Article
ISSN
0261-8028

No coin nor oath required. For personal study only.


๐Ÿ“œ SIMILAR VOLUMES


Synchrotron tomography of porosity in si
โœ T. Link; S. Zabler; A. Epishin; A. Haibel; M. Bansal; X. Thibault ๐Ÿ“‚ Article ๐Ÿ“… 2006 ๐Ÿ› Elsevier Science ๐ŸŒ English โš– 550 KB

Porosity in the single-crystal nickel-base superalloys CMSX-6, SRR99, CMSX-4 and CMSX-10 was investigated by synchrotron X-ray tomography, supplying information about the three dimensional distribution of pores and a statistical database of pore sizes and shapes. Tomography investigations were compl

The elastic constants of nickel-copper a
โœ S.G Epstein; O.N Carlson ๐Ÿ“‚ Article ๐Ÿ“… 1965 ๐Ÿ› Elsevier Science โš– 554 KB

The elastic constants of single crystals of the nickel-copper alloy system were determined by an ultrasonic pulse-echo technique. The elastic constants are proportional to the nickel concentration up to 70 at. 'A nickel at room temperature. Above this concentration where the alloys are ferromagnetic