๐”– Bobbio Scriptorium
โœฆ   LIBER   โœฆ

APFIM characterization of single-crystal PWA 1480 nickel-base superalloy

โœ Scribed by M.K Miller; R Jayaram; L.S Lin; A.D Cetel


Publisher
Elsevier Science
Year
1994
Tongue
English
Weight
707 KB
Volume
76-77
Category
Article
ISSN
0169-4332

No coin nor oath required. For personal study only.


๐Ÿ“œ SIMILAR VOLUMES


Synchrotron tomography of porosity in si
โœ T. Link; S. Zabler; A. Epishin; A. Haibel; M. Bansal; X. Thibault ๐Ÿ“‚ Article ๐Ÿ“… 2006 ๐Ÿ› Elsevier Science ๐ŸŒ English โš– 550 KB

Porosity in the single-crystal nickel-base superalloys CMSX-6, SRR99, CMSX-4 and CMSX-10 was investigated by synchrotron X-ray tomography, supplying information about the three dimensional distribution of pores and a statistical database of pore sizes and shapes. Tomography investigations were compl