As were heat treated over the range 250-500~C, and chemical depth profiles were obtained by measuring the surface composition with Auger electron spectroscopy while ion milling. Platinum films were 125-9000A thick. When Pt/GaAs was heated hz vacuum, the Pt-GaAs interaction initiated with a rapid mig