Thermal Conductivity of28Si from 80 to 300 K
โ Scribed by A. V. Gusev; A. M. Gibin; O. N. Morozkin; V. A. Gavva; A. V. Mitin
- Book ID
- 110401570
- Publisher
- SP MAIK Nauka/Interperiodica
- Year
- 2002
- Tongue
- English
- Weight
- 52 KB
- Volume
- 38
- Category
- Article
- ISSN
- 0020-1685
No coin nor oath required. For personal study only.
๐ SIMILAR VOLUMES
The thermal conductivity of several exfoliated graphites (Grafoil, Foam, and UCA R-ZYX graphite) has been measured in the range 2 to 300 K. The temperature dependence of the thermal conductivity is similar to that of near-single-crystal pyrolytic graphite, but the value is two orders of magnitude lo
The thermal diffusivity and thermal conductivity of as-deposited, annealed, and stress-annealed pyrolytic graphite have been measured at room temperature and over the range 1500-2700ยฐK. Values of the thermal conductivity parallel to the plane of deposition compare reasonably well with published resu