Thermal Conductivity of Silicon from 300 to 1400°K
✍ Scribed by Shanks, H. R.; Maycock, P. D.; Sidles, P. H.; Danielson, G. C.
- Book ID
- 120551119
- Publisher
- The American Physical Society
- Year
- 1963
- Tongue
- English
- Weight
- 547 KB
- Volume
- 130
- Category
- Article
- ISSN
- 0031-899X
No coin nor oath required. For personal study only.
📜 SIMILAR VOLUMES
The thermal conductivity of several exfoliated graphites (Grafoil, Foam, and UCA R-ZYX graphite) has been measured in the range 2 to 300 K. The temperature dependence of the thermal conductivity is similar to that of near-single-crystal pyrolytic graphite, but the value is two orders of magnitude lo