Five kinds of ceramics were used to evaluate the bending strength under three-point bending. The bending test was carried out at room temperature. The crack-healing behavior and the bending strength of the crack-healed specimens were investigated from room temperature to 1723 K. The bending strength
โฆ LIBER โฆ
The crack healing behavior of ZrO2/SiC composite ceramics with TiO2additive
โ Scribed by Nam, Ki Woo; Hwang, Jin Ryang
- Book ID
- 113099839
- Publisher
- Springer-Verlag
- Year
- 2012
- Tongue
- English
- Weight
- 501 KB
- Volume
- 26
- Category
- Article
- ISSN
- 1738-494X
No coin nor oath required. For personal study only.
๐ SIMILAR VOLUMES
Bending strength and crack-healing behav
โ
Hae Sook Kim; Mi Kyung Kim; Sun Bae Kang; Seok Hwan Ahn; Ki Woo Nam
๐
Article
๐
2008
๐
Elsevier Science
๐
English
โ 665 KB
In situ crack-healing behavior of Al2O3/
โ
Sung-Po Liu; Kotoji Ando; Byung-Soo Kim; Koji Takahashi
๐
Article
๐
2009
๐
Elsevier Science
๐
English
โ 745 KB
Strength recovery of machined Al2O3/SiC
โ
M. ONO; W. NAKAO; K. TAKAHASHI; K. ANDO
๐
Article
๐
2007
๐
John Wiley and Sons
๐
English
โ 579 KB
Crack-healing behavior and bending stren
โ
Ki Woo Nam; Mi Kyung Kim; Sung Won Park; Seok Hwan Ahn; Jong Soon Kim
๐
Article
๐
2007
๐
Elsevier Science
๐
English
โ 621 KB
Si 3 N 4 /SiC composite ceramics were sintered in order to investigate their bending strength behavior after crack-healing. Y 2 O 3 and TiO 2 powder was added as sintering additives to enhance it's sintering property. A three-point bending specimen was cut out from sintered plates. About 100 m semi-
Crack Healing Behavior of SiC Whisker Re
โ
Hu, Jun Feng; Zhu, Shi Jie; Wang, Wen Xue; Nakahara, Yukiko
๐
Article
๐
2013
๐
Trans Tech Publications, Ltd.
๐
English
โ 398 KB
Crack healing, reopening and thermal exp
โ
Hyung Chul Kim; Kee Sung Lee; Oh Seong Kweon; Christos G. Aneziris; Ik Jin Kim
๐
Article
๐
2007
๐
Elsevier Science
๐
English
โ 814 KB