Bending strength and crack-healing behavior of Al2O3/SiC composites ceramics
β Scribed by Hae Sook Kim; Mi Kyung Kim; Sun Bae Kang; Seok Hwan Ahn; Ki Woo Nam
- Publisher
- Elsevier Science
- Year
- 2008
- Tongue
- English
- Weight
- 665 KB
- Volume
- 483-484
- Category
- Article
- ISSN
- 0921-5093
No coin nor oath required. For personal study only.
β¦ Synopsis
Five kinds of ceramics were used to evaluate the bending strength under three-point bending. The bending test was carried out at room temperature. The crack-healing behavior and the bending strength of the crack-healed specimens were investigated from room temperature to 1723 K. The bending strength of Al 2 O 3 /SiC composite ceramics is higher than that of Al 2 O 3 monolithic. Al 2 O 3 /SiC composite ceramics could completely heal semicircular cracks with diameters 100 m. The bending strength of Al 2 O 3 /SiC composite ceramics significantly increased after heat treatment at 1573 K for 1 h in air. The crack-healing ability of Al 2 O 3 /SiC composite ceramics was the best in additive powder 3 wt.% Y 2 O 3 .
π SIMILAR VOLUMES
Si 3 N 4 /SiC composite ceramics were sintered in order to investigate their bending strength behavior after crack-healing. Y 2 O 3 and TiO 2 powder was added as sintering additives to enhance it's sintering property. A three-point bending specimen was cut out from sintered plates. About 100 m semi-
The self-crack-healing ability was systematically studied using flexural strength measurement of beams containing a semi-elliptical surface crack made by Vickers indenter. Beams of Al 2 O 3 /SiC ceramic nanocomposite with a good self-crack-healing ability predetermined for four-point and three-point
## Abstract The purpose of this study is to investigate the subcritical crack growth (SCG) behavior of aluminaβglass dental composites. Aluminaβglass composites were fabricated by infiltrating molten glass to porous alumina preforms. Rectangular bars of the composite were subject to dynamic loading