๐”– Bobbio Scriptorium
โœฆ   LIBER   โœฆ

Strength recovery of machined Al2O3/SiC composite ceramics by crack healing

โœ Scribed by M. ONO; W. NAKAO; K. TAKAHASHI; K. ANDO


Book ID
109015342
Publisher
John Wiley and Sons
Year
2007
Tongue
English
Weight
579 KB
Volume
30
Category
Article
ISSN
8756-758X

No coin nor oath required. For personal study only.


๐Ÿ“œ SIMILAR VOLUMES


Bending strength and crack-healing behav
โœ Hae Sook Kim; Mi Kyung Kim; Sun Bae Kang; Seok Hwan Ahn; Ki Woo Nam ๐Ÿ“‚ Article ๐Ÿ“… 2008 ๐Ÿ› Elsevier Science ๐ŸŒ English โš– 665 KB

Five kinds of ceramics were used to evaluate the bending strength under three-point bending. The bending test was carried out at room temperature. The crack-healing behavior and the bending strength of the crack-healed specimens were investigated from room temperature to 1723 K. The bending strength

Fracture behaviour of Al2O3/SiC nanocomp
โœ Zdenek Chlup; Petr Flasar; Ando Kotoji; Ivo Dlouhy ๐Ÿ“‚ Article ๐Ÿ“… 2008 ๐Ÿ› Elsevier Science ๐ŸŒ English โš– 769 KB

The self-crack-healing ability was systematically studied using flexural strength measurement of beams containing a semi-elliptical surface crack made by Vickers indenter. Beams of Al 2 O 3 /SiC ceramic nanocomposite with a good self-crack-healing ability predetermined for four-point and three-point

Crack-healing behavior and bending stren
โœ Ki Woo Nam; Mi Kyung Kim; Sung Won Park; Seok Hwan Ahn; Jong Soon Kim ๐Ÿ“‚ Article ๐Ÿ“… 2007 ๐Ÿ› Elsevier Science ๐ŸŒ English โš– 621 KB

Si 3 N 4 /SiC composite ceramics were sintered in order to investigate their bending strength behavior after crack-healing. Y 2 O 3 and TiO 2 powder was added as sintering additives to enhance it's sintering property. A three-point bending specimen was cut out from sintered plates. About 100 m semi-