Temperature-dependent Fourier transform infrared and differential scanning calorimetry studies of zinc carboxylates

✍ Scribed by O. Berkesi; T. Katona; I. Dreveni; J.A. Andor; J. Mink


Book ID
108027811
Publisher
Elsevier Science
Year
1995
Tongue
English
Weight
574 KB
Volume
8
Category
Article
ISSN
0924-2031

No coin nor oath required. For personal study only.


πŸ“œ SIMILAR VOLUMES


Degradation behavior of an ultraviolet a
✍ Adriane Ludwick; Heshmat Aglan; Mohamed O. Abdalla; Maria Calhoun πŸ“‚ Article πŸ“… 2008 πŸ› John Wiley and Sons 🌐 English βš– 213 KB πŸ‘ 2 views

## Abstract The degradation behavior of an elastomeric polyurethane (PU) was investigated with accelerated ultraviolet (UV) and hygrothermal (HT) techniques. Samples were subjected to UV exposure and HT conditions for 3 or 5 months and were removed in 1‐month intervals from the test chambers. Their