Fourier transform infrared spectroscopy and differential scanning calorimetry studies of fatty acid homogeneous ceramide 2
β Scribed by Hui-Chen Chen; Richard Mendelsohn; Mark E. Rerek; David J. Moore
- Book ID
- 117047685
- Publisher
- Elsevier Science
- Year
- 2000
- Tongue
- English
- Weight
- 719 KB
- Volume
- 1468
- Category
- Article
- ISSN
- 0005-2736
No coin nor oath required. For personal study only.
π SIMILAR VOLUMES
## Abstract The degradation behavior of an elastomeric polyurethane (PU) was investigated with accelerated ultraviolet (UV) and hygrothermal (HT) techniques. Samples were subjected to UV exposure and HT conditions for 3 or 5 months and were removed in 1βmonth intervals from the test chambers. Their
The staling of bread has previously been studied by differential scanning calorimetry and by simple rheological measurements. In this collaborative study, two spectroscopic techniques (Fourier transform mid infrared spectroscopy and near infrared reflectance spectroscopy) have been used in addition