๐”– Bobbio Scriptorium
โœฆ   LIBER   โœฆ

Synthesis of Nested Coaxial Multiple-Walled Nanotubes by Atomic Layer Deposition

โœ Scribed by Gu, Diefeng; Baumgart, Helmut; Abdel-Fattah, Tarek M.; Namkoong, Gon


Book ID
127105183
Publisher
American Chemical Society
Year
2010
Tongue
English
Weight
45 KB
Volume
4
Category
Article
ISSN
1936-0851

No coin nor oath required. For personal study only.


๐Ÿ“œ SIMILAR VOLUMES