✦ LIBER ✦
Atomic Layer Deposition of ZnO on Multi-walled Carbon Nanotubes and Its Use for Synthesis of CNT–ZnO Heterostructures
✍ Scribed by X. L. Li; C. Li; Y. Zhang; D. P. Chu; W. I. Milne; H. J. Fan
- Publisher
- Springer-Verlag
- Year
- 2010
- Tongue
- English
- Weight
- 408 KB
- Volume
- 5
- Category
- Article
- ISSN
- 1931-7573
No coin nor oath required. For personal study only.