Two polyurethane blends-poly(carbonate urethane)/poly (vinyl alcohol) [PCU/PVA] and the aliphatic poly(ether urethane) (Tecoflex@)/poly(pentanedioic acid mono-4-(acryl-oy1oxy)butyl ester) [Tecoflex@/COOH]-were surface-modified. Poly(viny1 alcohol) [ PVA] and poly(4-hydroxybutyl acrylate) [PHBA] were
Surface analysis of PP/EVA blends modified with amino acids for biomedical applications
✍ Scribed by K. Schroeder; D. Klee; H. Höcker; A. Leute; A. Benninghoven; C. Mittermayer
- Publisher
- John Wiley and Sons
- Year
- 1995
- Tongue
- English
- Weight
- 695 KB
- Volume
- 58
- Category
- Article
- ISSN
- 0021-8995
No coin nor oath required. For personal study only.
📜 SIMILAR VOLUMES
A procedure which allows quantitative determination of the amino acid composition of stained proteins separated by sodium dodecyl sulfate (SDS)-gel electrophoresis using ninhydrin is described. The Coomassie-protein-SDS complex extracted from the gel is dialyzed, lyophylized, and subjected to amino
## Abstract Analysis of underivatized amino acids is challenging regarding the separation as well as the detection of these small polar analytes. Hydrophilic interaction LC using a 2.1×150 mm ZIC^®^ (ZIC, zwitterionic)‐hydrophilic interaction LC from SeQuant as stationary phase with 1% v/v formic a