Stress corrosion of stainless steels in aerated steam

✍ Scribed by V. A. Shuvalov; V. V. Gerasimov


Publisher
Springer
Year
1969
Tongue
English
Weight
195 KB
Volume
4
Category
Article
ISSN
1573-885X

No coin nor oath required. For personal study only.


πŸ“œ SIMILAR VOLUMES


Environmental aspects of stress corrosio
✍ Ing. B. Eremi; V. A. Maričev πŸ“‚ Article πŸ“… 1979 πŸ› John Wiley and Sons 🌐 German βš– 323 KB πŸ‘ 1 views

## Abstract Stress corrosion crack velocity and stress corrosion threshold stress intensity have been measured for 18Cr–10Ni–0,5Ti stainless steel in relation to environmental variations. These studies showed that both stage I and stage II growth rate dependence on K are influenced by environmental