๐”– Bobbio Scriptorium
โœฆ   LIBER   โœฆ

Stress corrosion cracking of bone implants

โœ Scribed by G. Bombara; M. Cavallini


Book ID
115845955
Publisher
Elsevier Science
Year
1977
Tongue
English
Weight
723 KB
Volume
17
Category
Article
ISSN
0010-938X

No coin nor oath required. For personal study only.


๐Ÿ“œ SIMILAR VOLUMES


Stress-corrosion Cracking of Aluminium
โœ JACOBS, A. J. ๐Ÿ“‚ Article ๐Ÿ“… 1966 ๐Ÿ› Nature Publishing Group ๐ŸŒ English โš– 296 KB
Stress-corrosion cracking of copper
โœ E.N. Pugh; W.G. Montague; A.R.C. Westwood ๐Ÿ“‚ Article ๐Ÿ“… 1966 ๐Ÿ› Elsevier Science ๐ŸŒ English โš– 742 KB
People and Stress Corrosion Cracking