Stress Corrosion Cracking of Magnesium A
โœ Andrej Atrens; Nicholas Winzer; Wolfgang Dietzel ๐Ÿ“‚ Article ๐Ÿ“… 2011 ๐Ÿ› John Wiley and Sons ๐ŸŒ English โš– 880 KB
A note on stress corrosion cracking rate
โœ S. Mostovoy; H.R. Smith; R.G. Lingwall; E.J. Ripling ๐Ÿ“‚ Article ๐Ÿ“… 1971 ๐Ÿ› Elsevier Science ๐ŸŒ English โš– 736 KB

The dependence of cracking rate, ii, on applied stress intensity factor, K,,, was measured in either salt water, or distilled water for the following steels: 300M, 250 grade maraging and the 9 Ni-4 Co-O.45 C. all heat treated to tensile strengths between 200 and 250 ksi. For each of these there was