## Abstract Stress corrosion crack velocity and stress corrosion threshold stress intensity have been measured for 18Crβ10Niβ0,5Ti stainless steel in relation to environmental variations. These studies showed that both stage I and stage II growth rate dependence on K are influenced by environmental
The corrosion assisted stress crack growth rate of 304L stainless steel welds, was determined by the rising displacement test method. The experiments were carried out in a Boiling Water Reactor (BWR) environment, using a refreshed autoclave loop system at 288 C and 8 MPa of pressure. Pre-fatigued CT