## Abstract Edge‐loading generates higher wear rates in ceramic‐on‐ceramic total hip prosthesis (THP). To investigate the friction coefficient (FC) in these conditions, three alumina ceramic (Biolox Forte) 32 mm‐diameter components were tested using a hip friction simulator. The cup was positioned
Spectral characterization of squeaking in ceramic-on-ceramic total hip arthroplasty: Comparison of in vitro and in vivo values
✍ Scribed by Elhadi Sariali; Zhongmin Jin; Todd Stewart; John Fisher
- Publisher
- Elsevier Science
- Year
- 2011
- Tongue
- English
- Weight
- 298 KB
- Volume
- 30
- Category
- Article
- ISSN
- 0736-0266
No coin nor oath required. For personal study only.
✦ Synopsis
Abstract
Squeaking is a cause for concern in total hip arthroplasty (THA). However, the definition of this sound remains vague. Our goals were to characterize spectrally the squeaking in vitro under lubricated conditions and to compare the in vitro frequencies to in vivo frequencies. Four patients, who presented with a squeaking after ceramic‐on‐ceramic THA were investigated. In addition, 3 alumina ceramic 32 mm diameter components were tested in vitro under edge loading conditions using a friction simulator. Tests were conducted under lubricated conditions without and with the addition of a third body alumina particle. In vitro, no squeaking occurred under edge loading conditions. However, with the addition of a third body particle in the contact region, squeaking was obtained; the dominant frequency was 2.6 kHz. In vivo, the main recorded sound frequencies were: 2.3, 2.24, and 2.46 kHz for squeakers during walking and 1.45 kHz for a squeaker rising from a bent position. The in vivo recordings had a dominant frequency similar to, but slightly lower than, the in vitro values. Two types of squeaking were found in vivo and characterized spectrally. The rising squeaker had intermittent squeaking corresponding to a lower fundamental frequency compared to the walking squeakers. This finding suggests two different mechanism of squeaking. © 2011 Orthopaedic Research Society Published by Wiley Periodicals, Inc. J Orthop Res 30:185–189, 2012
📜 SIMILAR VOLUMES
## Abstract We investigated articular bearing surfaces retrieved from three patients with ceramic‐on‐ceramic total hip arthroplasties using high‐quality alumina. The duration of implantation was 3.5, 3.0, and 2.5 years, respectively. Dislocation of the hip joint after implantation did not occur in
Wear of yttria-zirconia (zirconia) in the femoral head was investigated in mature mongrel dogs weighing 10 to 13 kg. Two dogs, which were used as a control group, were sacrificed 18 months after implantation of the uncemented modular hip system with an alumina ceramic (alumina) femoral head. A zirco
Protein adsorption affects the function of cells and determines the bioactivity of biomaterial implants. Surface structure and properties of materials determine the behavior of protein adsorption. In the present study, two biphasic calcium-phosphate ceramics (BCPs) with different surface structures
## Abstract In this study, we addressed whether Bone Sialoprotein (BSP) coating of various substrates could enhance the __in vitro__ osteogenic differentiation and __in vivo__ bone formation capacity of human Bone Marrow Stromal Cells (BMSC). Moreover, we tested whether synthetic polymer‐based poro