𝔖 Bobbio Scriptorium
✦   LIBER   ✦

Simultaneous chemical vapour deposition of carbon and uranium

✍ Scribed by S. Marinković; Ć. Sužnjević; I. Dežarov


Publisher
Elsevier Science
Year
1969
Tongue
English
Weight
428 KB
Volume
33
Category
Article
ISSN
0022-3115

No coin nor oath required. For personal study only.


📜 SIMILAR VOLUMES


Carbon/carbon composites prepared by che
✍ S. Marinković; S. Dimitruević 📂 Article 📅 1985 🏛 Elsevier Science 🌐 English ⚖ 921 KB

This paper summarizes the results of the authors' work on C/C composites prepared by chemical vapour deposition (CVD), using propylene as a source of carbon and various substrates (cellulose carbon, natural graphite, different grades of carbon fibres bonded by phenolic or CVD carbon). The equations

Chemical vapour deposition of silanes
✍ Ulf Jönsson; Göran Olofsson; Magnus Malmqvist; Inger Rönnberg 📂 Article 📅 1985 🏛 Elsevier Science 🌐 English ⚖ 540 KB
Simultaneous pyrolytic deposition of car
✍ S. Marinković; Č. Sužnjević; I. Dežarov 📂 Article 📅 1969 🏛 Elsevier Science 🌐 English ⚖ 883 KB

a-Boron-containing pyrocarbons were prepared at temperatures 1400-1650°C by simultaneous pyrolytic deposition from gas mixtures containing CH, and BCI, on an induction heated graphite substrate. The deposits thus prepared with boron content in the range O-3 per cent (w/o) were investigated using X-r

The Chemical Vapour Deposition of Tantal
✍ Drs. D. J. Jerreat; Rees D. Rawlings 📂 Article 📅 1974 🏛 John Wiley and Sons 🌐 English ⚖ 485 KB

## Abstract The effect of the total pressure, feed temperature, deposition temperature, and reaction tube inclination and geometry on the chemical vapour deposition of tantalum from the pentaiodide has been investigated. Transport rates as high as 350 mg hr^−1^ were achieved in inclined tubes of sp