Porous silk fibroin materials, with average pore size 10 Ο³ 300 m, pore density 1 Ο³ 2000/mm 2 , and porosity 35 Ο³ 70%, were prepared by freeze drying aqueous solution of silk fibroin obtained by dissolving silk fibroin in ternary solvent CaCl 2 β CH 3 CH 2 OH β H 2 O. Pore size distribution of such m
Silk Fibroin Based Porous Materials
β Scribed by Zhang, Qiang; Yan, Shuqin; Li, Mingzhong
- Book ID
- 121293579
- Publisher
- MDPI AG
- Year
- 2009
- Tongue
- English
- Weight
- 229 KB
- Volume
- 2
- Category
- Article
- ISSN
- 1996-1944
No coin nor oath required. For personal study only.
π SIMILAR VOLUMES
Silk fibroin solution was prepared by dissolving the silk fibroin in triad solvent CaCl 2 β CH 3 CH 2 OH β H 2 O. In this article we tested and analyzed the state of frozen silk fibroin solution and fine structure of freeze dried porous silk fibroin materials. The results indicated that the glass tr
## Abstract Fibers made of cellulose (CE) and silk fibroin (SF) are wet spun from solutions in __N__,__N__βdimethylacetamide containing 7% LiCl (w/w). Different coagulation baths (water and ethanol) and spinning conditions are used. By using water as the coagulant, a partial dissolution of SF occur