Radical Enhanced Atomic Layer Deposition of Titanium Dioxide
✍ Scribed by A. Niskanen; K. Arstila; M. Leskelä; M. Ritala
- Publisher
- John Wiley and Sons
- Year
- 2007
- Tongue
- English
- Weight
- 392 KB
- Volume
- 13
- Category
- Article
- ISSN
- 0948-1907
No coin nor oath required. For personal study only.
📜 SIMILAR VOLUMES
## Abstract In this paper, a method for the plasma‐enhanced (PE) atomic layer deposition (ALD) of palladium on air‐exposed, annealed poly(__p__‐xylylene) (Parylene‐N, or PPX) is presented. Palladium is successfully deposited on PPX at 80 °C using a remote, inductively coupled, hydrogen/nitrogen pla
## Abstract HfO~2~ films were grown by atomic layer deposition (ALD) from a new liquid precursor, Hf(ONEt~2~)~4~ and H~2~O, at temperatures between 250 °C and 350 °C on borosilicate glass and Si(100) substrates. The highest growth rate was achieved at 300 °C, whereas the growth was essentially slow