## Abstract The foundational data and rules of SUS304 corrosion in aqueous lithium bromide solution at 150โ200โยฐC have been investigated by means of weight loss in this paper. The Taguchi method was chosen to investigate the effects of variables on corrosion at higher temperature. Concentration of
Passivity and Pitting Susceptibility of type 304 Stainless Steel in Acidic Sulphate Solutions
โ Scribed by S. S. El-Egamy; W. A. Badawy; H. Shehata
- Publisher
- John Wiley and Sons
- Year
- 2001
- Tongue
- English
- Weight
- 158 KB
- Volume
- 32
- Category
- Article
- ISSN
- 0933-5137
No coin nor oath required. For personal study only.
๐ SIMILAR VOLUMES
## Abstract The inhibition effect of the extract of galbanum (__Ferula gummosa__ Boiss.) on the corrosion of 304 stainless steel in 2 M HCl solution was studied by weight loss measurements, Tafel polarization, and electrochemical impedance spectroscopy (EIS) methods. It was found that the inhibitio
The localised corrosion resistance (pitting and crevice corrosion) of two high alloy stainless steels, namely superduplex (SD) and superaustenitic (SA), has been studied in chloride-fluoride solutions at pH values ranging from 2 to 6.5. The pitting potential (E pit ) and crevice potential (E cre ) h
## Abstract The 00Cr18Ni10 stainless steel was examined before and after plasma nitriding in a 80%N~2~/20%H~2~ gas mixture at 425ยฐC for 30 h, resulting in the formation of a supersaturated solid solution of nitrogen in austenite (__S__ phase) with 12.9 wt.% N at the surface. Electrochemical measure
Positron annihilation lifetime and Doppler broadening measurements have been performed to study the early stage of fatigue in type 304 stainless steel at various positions of samples at room temperature. Both the average lifetime of positron and the S parameter have increased with increasing number
## Abstract In corrosion medium, metals can deform under tensile stress and form a new active surface with the anodic dissolution of the metals being accelerated. At the same time, the anodic dissolution may accelerate the deformation of the metals. The synergy can lead to crack nucleation and deve