Pitting corrosion transformation of SUS304 stainless steel in lithium bromide solution at high temperature

✍ Scribed by H.-X. Chen; X.-H. Ma; J.-B. Chen; S.-S. Bo


Publisher
John Wiley and Sons
Year
2009
Tongue
German
Weight
207 KB
Volume
60
Category
Article
ISSN
0947-5117

No coin nor oath required. For personal study only.

✦ Synopsis


Abstract

The foundational data and rules of SUS304 corrosion in aqueous lithium bromide solution at 150–200 °C have been investigated by means of weight loss in this paper. The Taguchi method was chosen to investigate the effects of variables on corrosion at higher temperature. Concentration of dissolved oxygen was controlled by keeping the vessel pressure at 1.3 kPa (absolute) before the experiment. The results showed that there was a transformation tendency from pitting corrosion to general corrosion and transition concentration of pitting and film corrosion decreased with increase in solution temperature. The adsorption, activity, and diffusivity of bromine ion led to different corrosion modalities.