Nickel foil was oxidized for 24 hr periods within the temperature range 307" to 442Β°C producing NiO fihns up to 3400 A thick maximum. A discontinuity in oxide growth is observed at the Curie temperat,ure (353Β°C). Data obtained at 390", 394" and 405Β°C as a function of time show that a two-stage oxi
Oxidation of nickel-cobalt alloys in the range of Curie temperatures
β Scribed by W.W Smeltzer
- Publisher
- Elsevier Science
- Year
- 1959
- Weight
- 932 KB
- Volume
- 7
- Category
- Article
- ISSN
- 0001-6160
No coin nor oath required. For personal study only.
π SIMILAR VOLUMES
Kinetic and crystallographic observations on the natural and stress-induced transformations in single crystals of cobalt and cobalt-nickel alloys have oonhrmed the martensitic nature of the change. The shape deformation has been measured for the stress-induced transformation in alloys; the habit pla
## Abstract Anomalies in the Arrhenius plot of the thin film (10^2^β10^5^ Γ ) oxidation of nickel and iron at the Curie temperature are discussed. Amongst the various theories, a mechanism which takes into account the importance of both the surfaceβstate charge at the metal/oxide interface and the s