Nanoindentation of GaSe thin films

✍ Scribed by Sheng-Rui Jian, Shin-An Ku, Chih-Wei Luo, Jenh-Yih Juang


Book ID
119906032
Publisher
Springer-Verlag
Year
2012
Tongue
English
Weight
526 KB
Volume
7
Category
Article
ISSN
1931-7573

No coin nor oath required. For personal study only.