Nanoindentation and Raman spectroscopy studies of boron carbide single crystals

✍ Scribed by Domnich, Vladislav; Gogotsi, Yury; Trenary, Michael; Tanaka, Takaho


Book ID
120511448
Publisher
American Institute of Physics
Year
2002
Tongue
English
Weight
264 KB
Volume
81
Category
Article
ISSN
0003-6951

No coin nor oath required. For personal study only.


πŸ“œ SIMILAR VOLUMES


ChemInform Abstract: Raman Spectroscopy
✍ Dimitar D. Radev; Boriana Mihailova; Ludmil Konstantinov πŸ“‚ Article πŸ“… 2010 πŸ› John Wiley and Sons βš– 28 KB πŸ‘ 1 views

## Abstract ChemInform is a weekly Abstracting Service, delivering concise information at a glance that was extracted from about 100 leading journals. To access a ChemInform Abstract of an article which was published elsewhere, please select a β€œFull Text” option. The original article is trackable v

Raman spectroscopy study of , , and crys
✍ Yunlong Cui; Utpal N. Roy; Pijush Bhattacharya; Adrian Parker; Arnold Burger; Jo πŸ“‚ Article πŸ“… 2010 πŸ› Elsevier Science 🌐 English βš– 449 KB

AgGaSe 2 , AgGa 0.9 In 0.1 Se 2 , and AgGa 0.8 In 0.2 Se 2 single crystals grown by the horizontal Bridgman technique were studied utilizing Raman spectroscopy excited with 633-and 784-nm lasers at temperatures varied from 77 to 300 K. The resonant Raman scattering associated with a transition from

Raman studies of sodium fluoroborate sin
✍ Murray H. Brooker πŸ“‚ Article πŸ“… 1993 πŸ› John Wiley and Sons 🌐 English βš– 538 KB

## Abstract Raman spectra of oriented single crystals of NaBF~4~ were measured at 77 and 298 K. The number of bands and the intensities were in excellent agreement with the unit cell group predictions for the known crystal structure, __D__, __Z__ = 2. The results for the Ξ½~1~, Ξ½~2~ and Ξ½~4~ regions