Influence of ultrasound on pitting corrosion and crevice corrosion of SUS304 stainless steel in chloride sodium aqueous solution
โ Scribed by Rongguang Wang
- Book ID
- 116384888
- Publisher
- Elsevier Science
- Year
- 2008
- Tongue
- English
- Weight
- 389 KB
- Volume
- 50
- Category
- Article
- ISSN
- 0010-938X
No coin nor oath required. For personal study only.
๐ SIMILAR VOLUMES
The localised corrosion resistance (pitting and crevice corrosion) of two high alloy stainless steels, namely superduplex (SD) and superaustenitic (SA), has been studied in chloride-fluoride solutions at pH values ranging from 2 to 6.5. The pitting potential (E pit ) and crevice potential (E cre ) h
## Abstract The foundational data and rules of SUS304 corrosion in aqueous lithium bromide solution at 150โ200โยฐC have been investigated by means of weight loss in this paper. The Taguchi method was chosen to investigate the effects of variables on corrosion at higher temperature. Concentration of