𝔖 Bobbio Scriptorium
✦   LIBER   ✦

Influence of interaction between multiple cracks on stress corrosion crack propagation

✍ Scribed by Masayuki Kamaya; Nobuo Totsuka


Book ID
117085864
Publisher
Elsevier Science
Year
2002
Tongue
English
Weight
392 KB
Volume
44
Category
Article
ISSN
0010-938X

No coin nor oath required. For personal study only.


πŸ“œ SIMILAR VOLUMES


Influence of microcompositional gradient
✍ G.L. Berry Jr.; D.L. Olson; D.K. Matlock πŸ“‚ Article πŸ“… 1991 πŸ› Elsevier Science 🌐 English βš– 446 KB

Stress corrosion cracking in compositionally non-uniform systems is addressed. Of special interest is the preferred direction of crack propagation in stress-corroded weld metal. Solidified structures of a cast austenitic stainless steel designed to simulate a solidified weld structure were homogeniz