๐”– Bobbio Scriptorium
โœฆ   LIBER   โœฆ

Effect of Crack-Tip Stresses on Stress Corrosion Cracking Behavior

โœ Scribed by D. Kujawski; K. Sadananda


Book ID
107444174
Publisher
The Minerals, Metals & Materials Society
Year
2010
Tongue
English
Weight
570 KB
Volume
42
Category
Article
ISSN
1073-5623

No coin nor oath required. For personal study only.


๐Ÿ“œ SIMILAR VOLUMES


Crack-tip stresses and their effect on s
โœ S. Stoychev; D. Kujawski ๐Ÿ“‚ Article ๐Ÿ“… 2008 ๐Ÿ› Elsevier Science ๐ŸŒ English โš– 608 KB

In this paper, analytical and numerical simulations of the crack-tip stresses are presented. Analytical calculations are performed utilizing modified Rice and elastic equations. 2D finite element analyses (FEA) are conducted in parallel using ANSYS. Results from both methods are compared and discuss