𝔖 Bobbio Scriptorium
✦   LIBER   ✦

Influence of adherend surface preparation on bond durability

✍ Scribed by Rider, A. N.; Olsson-Jacques, C. L.; Arnott, D. R.


Publisher
John Wiley and Sons
Year
1999
Tongue
English
Weight
629 KB
Volume
27
Category
Article
ISSN
0142-2421

No coin nor oath required. For personal study only.

✦ Synopsis


Work presented in this paper focuses on the critical aspects of the surface preparation of aluminium employed for the manufacture of aluminium-epoxy joints. The surface preparation procedure examined is currently employed by the Royal Australian Airforce (RAAF) for repairs requiring metal-to-adhesive bonding. The influence of each step in the surface preparation on the bond durability performance of the adhesive joint is examined by a combination of methods. Double-cantilever wedge-style adhesive joints are loaded in mode 1 opening and exposed to a humid environment. Together with analysis of the adherend and joint failure surfaces, the results show conclusively that adhesive bond durability is sensitive to the presence of contaminant and the roughness of the adherend surface. The presence of contaminant can interfere with the effectiveness of an organosilane coupling agent as a durability improver. A two-step bond degradation model was developed to describe qualitatively the observed bond durability performance and fracture data.


πŸ“œ SIMILAR VOLUMES


Effect of surface preparation on the dur
✍ E. M. Meier Jackson; N. M. Yanar; M. C. Maris-Jakubowski; K. Onal-Hance; G. H. M πŸ“‚ Article πŸ“… 2008 πŸ› John Wiley and Sons 🌐 German βš– 565 KB

## Abstract A principal concern with alumina‐forming coatings for high‐temperature oxidation protection and bond coats (BCs) for ceramic thermal barrier coatings (TBCs) used in gas turbines is the spalling of the alumina scales during service. This paper describes the effects of BC surface preparat

The effects of adherend on the strength
✍ Tezcan Sekercioglu; Cemal Meran πŸ“‚ Article πŸ“… 2004 πŸ› Elsevier Science βš– 261 KB

The strength of adhesively bonded cylindrical components was affected by the various factors, which are diametrical clearance, type of assembly, type of adherend, operating temperature, loading type, surface roughness, etc. In this study, the effect of three different adherend (steel, bronze and alu