Grain refinement of superalloy IN718C by the addition of inoculants

โœ Scribed by Yuhua Xiong; Xiu Ying Wei; Jun Du; Aimin Yang; Lin Liu; Daben Zeng


Book ID
107440577
Publisher
The Minerals, Metals & Materials Society