Grain refinement of superalloy K4169 by addition of refiners: cast structure and refinement mechanisms

✍ Scribed by Lin Liu; Taiwen Huang; Yuhua Xiong; Aimin Yang; Zhilong Zhao; Rong Zhang; Jinshan Li