๐”– Bobbio Scriptorium
โœฆ   LIBER   โœฆ

Grain refinement of superalloy IN100 under the action of rotary magnetic fields and inoculants

โœ Scribed by Wenzhong Jin; Fudong Bai; Tingju Li; Guomao Yin


Book ID
113791546
Publisher
Elsevier Science
Year
2008
Tongue
English
Weight
697 KB
Volume
62
Category
Article
ISSN
0167-577X