𝔖 Bobbio Scriptorium
✦   LIBER   ✦

Electrical and Optical Properties of ZnO Processed by Atomic Layer Deposition in Inverted Polymer Solar Cells †

✍ Scribed by Cheun, Hyeunseok; Fuentes-Hernandez, Canek; Zhou, Yinhua; Potscavage, William J.; Kim, Sung-Jin; Shim, Jaewon; Dindar, Amir; Kippelen, Bernard


Book ID
121231179
Publisher
American Chemical Society
Year
2010
Tongue
English
Weight
305 KB
Volume
114
Category
Article
ISSN
1932-7447