Structural and Electrical Properties of
โ
Do-Joong Lee; Hyun-Mi Kim; Jang-Yeon Kwon; Hyoji Choi; Soo-Hyun Kim; Ki-Bum Kim
๐
Article
๐
2010
๐
John Wiley and Sons
๐
English
โ 515 KB