𝔖 Bobbio Scriptorium
✦   LIBER   ✦

Effect of copolymer mixing on elongation property of as-spun PET fibers

✍ Scribed by Tae Hwan Oh


Publisher
John Wiley and Sons
Year
2006
Tongue
English
Weight
330 KB
Volume
101
Category
Article
ISSN
0021-8995

No coin nor oath required. For personal study only.

✦ Synopsis


Abstract

The change of elongation property in the melt spinning process of polyethylene terephthalate (PET) fibers, mixed with small amount of additive copolymer less than 5% by weight, was studied. The additive polymer was synthesized to improve the extensibility of matrix PET in the spinning process. The amount, molecular weight of additive polymer, and spinning conditions were changed to investigate the extensibility of as‐spun fibers. Experimental results show that the blend of copolymer improves the extensibility of as‐spun PET fibers. The elongation at break of as‐spun fibers increases with molecular weight and amount of additive polymer. The additive polymer prevents the fiber orientation and this causes the increase of extensibility of as‐spun fibers. © 2006 Wiley Periodicals, Inc. J Appl Polym Sci 101: 1426–1431, 2006


📜 SIMILAR VOLUMES


Effect of jet stretch on polyacrylonitri
✍ Bao-Hua Ji; Cheng-Guo Wang; Yan-Xiang Wang 📂 Article 📅 2006 🏛 John Wiley and Sons 🌐 English ⚖ 382 KB 👁 2 views

## Abstract In this article, the effect of jet stretch ratio on the extrudate die‐swell effect of polyacrylonitrile spinning solution and the structure and properties of as‐spun fibers was systematically analyzed by means of X‐ray diffraction (XRD), electron microprobe analysis, and the measurement

Effect of process parameters on properti
✍ Marja Rissanen; Arja Puolakka; Terttu Hukka; Ville Ellä; Pertti Nousiainen; Minn 📂 Article 📅 2009 🏛 John Wiley and Sons 🌐 English ⚖ 198 KB 👁 2 views

## Abstract Poly(L,D‐lactide) [P(L,D)LA], LL/D ratio 96/4, and poly(L,DL‐lactide) [P(L,DL)LA], L/DL ratio 70/30, multifilament fibers were prepared by wet‐spinning and the effects of the spin draw ratio and the coagulant on the morphological, thermal, and mechanical properties of the filaments were

Effect of hot drawing on properties of w
✍ Marja Rissanen; Arja Puolakka; Terttu Hukka; Ville Ellä; Minna Kellomäki; Pertti 📂 Article 📅 2010 🏛 John Wiley and Sons 🌐 English ⚖ 421 KB 👁 2 views

## Abstract Polylactide stereocopolymer multifilament fibers were prepared by wet spinning and subsequent hot drawing. The stereocopolymers were poly‐(L,D‐lactide) [P(L,D)LA], L/D ratio 96/4, and poly‐(L,DL‐lactide) [P(L,DL)LA], L/DL ratio 70/30. They were dissolved in dichloromethane and coagulate

Effect of protein-loading on properties
✍ Marja Rissanen; Arja Puolakka; Niina Ahola; Aaron Tonry; Yury Rochev; Minna Kell 📂 Article 📅 2010 🏛 John Wiley and Sons 🌐 English ⚖ 192 KB 👁 2 views

## Abstract Protein‐loaded multifilament fibers were fabricated by the wet‐spinning method. The polymers which were tested included poly(L,D‐lactide) [P(L,D)LA], L/D ratio 96/4 and poly(L,DL‐lactide) [P(L,DL)LA], L/DL ratio 70/30. The polymers were dissolved in dichloromethane and bovine serum albu