๐”– Bobbio Scriptorium
โœฆ   LIBER   โœฆ

Creep-rupture strength of a Ni-base superalloy at 1400 K

โœ Scribed by Whittenberger, J.Daniel; Nathal, Michael V.; Book, Patricia O.


Book ID
122452148
Publisher
Elsevier Science
Year
1993
Weight
439 KB
Volume
28
Category
Article
ISSN
0956-716X

No coin nor oath required. For personal study only.


๐Ÿ“œ SIMILAR VOLUMES


Creep of a co-rich Ni base superalloy
โœ Merabtine, R.; Bertrand, C.; Dallas, J.-P.; Devaud-Rzepski, J.; Trichet, M.-F.; ๐Ÿ“‚ Article ๐Ÿ“… 1990 ๐Ÿ› Elsevier Science โš– 459 KB
Creep of PE-10 nickel-base superalloy at
โœ A. J. Marzocca; A. C. Picasso ๐Ÿ“‚ Article ๐Ÿ“… 1994 ๐Ÿ› Springer ๐ŸŒ English โš– 853 KB

Creep data, at 973 K and stresses between 355 and 512 MPa, in flat specimens of PE-IO nickel-base superalloy are reported. The data have been interpreted in terms of a constitutive equation based on a creep model involving dislocation climb and cross-slip over the strengthening phase. Strain-rate se